1.4116 Approximate Comparative Table
1.4116 Approximate Comparative Table- Meterial no. 1.4116 to EN 10 088-2
Chemical Composition (in % by weight) i)
Mechanical Properties (Transverse Samples) At Room Temp.ii) to EN 10 088-2
ii) Hardened and tempered approx. 55 HRC. Calculating tensile strength from hardness is subject to wide fluctuations.
D (DIN/EN) | X50 CrMoV15 |
USA (ASTM) | - |
Japan | - |
CIS | - |
Chemical Composition (in % by weight) i)
C | Cr | Mn | V | |
Min. | 0.45 | 14.0 | 0.5 | 0.1 |
Max. | 0.55 | 15.0 | 0.8 | 0.2 |
Mechanical Properties (Transverse Samples) At Room Temp.ii) to EN 10 088-2
Dimensions range |
Rm (tensile strength) N/mm2 |
A5 (elongation) % |
A80 (elongation) % |
Hardness HB |
Cold-rolled strip s≦ 8mm Hot-rolled strip s≦ 13.5mm |
Max. 850 | ≧ 12 | ≧ 12 | ≦ 280 |